09 Nov 2015 - impact modifiers usage,impact-modifiers-liquids,plastic impact modifiers




Usage: just add when mixing. First mix LIQUID form jindaquan impact modifiers with the plastic raw materials for 15-20 minutes, after mixed even,put them into the plastic bags (also could leave them in the mixing bucket) ,placed them for 45 to 60 minutes to let the chemical reaction fully worked, then heat and roast them for extrusion, injection molding or blow molding. (if there is agglomeration, please pat it loose with a hard object or use the blender to stir it scattered.).


Notes:  

To test the results of adding ARGIOPE® impact modifiers , please wait for at least 24 HOURS after extrusion, injection molding or blow molding , for the effect is much more obvious at that time